All corrosion of iron at normal ambient conditions is - -an electrochemical process
-The cathode of a corrosion cell - -has an opposite electrical polarity to the anode
-Based on the galvanic series presented in the NACE CIP Level 1 Manual, which three
can be used effectively as galvanic anodes for carbon steel? - -Zinc, aluminum,
magnesium
-A corrosion inhibitor is a substance that, when added to an environment - -decreases
the rate of corrosion
-A decrease in temperature will generally cause the corrosion rate to - -decrease
-The electrolyte is the solution that carries (conducts) - -the anion, and the cations
-While oxidation occurs at the anode, reduction occurs at the cathode - -true
-The four elements of a corrosion cell are anode, the cathode, the electrode, and the
metallic pathway - -False
-The anode is the - -part of the metal that corrodes
-General corrosion is described as - -uniform loss of thickness over the exposed surface
-In order to reach consensus and to resolve conflict on the job, the NACE Inspector's
preferred course of action is to - -actively listen and endeavor to understand the
postions of others.
-A proper coating specification should contain information regarding - -surface
preparation standards, safety, locations to be coated
-According to the NACE attestation, it's OK to accept a gift from a contractor as long as
the gift is below the value identified in your company policy. - -false
-If an inspector finds discrepancies between the specification and the coating
manufacturers technical data sheet, the preferred coarse of action is to - -seek written
clarification from the specifier
-All of the following are generally included within inspection reports EXCEPT - -cost
information
, -Inspectors reports provide sufficient detail permitting the owner to evaluate - -
contractor's performance, inspector's performance, job progress, work interruptions
-When applying coatings, instruction regarding appropriate types of Personal
Protection Equipment (PPE) will always be found within the - -material safety data
sheet (MSDS) or safety data sheet (SDS)
-Material inventory report should contain all of the following EXCEPT - -overall cost of
materials
-Safety enforcement is one of the primary responsibilities of the coating inspector - -
false
-If the relative humidity is too high, solvent entrapment within the coating film may
occur. - -true
-The dew point is the - -temperature at which moisture condenses on a surface.
-Steel surface temperature reading should be taken - -at the actual work locations
-The coatings inspector must calibrate the magnetic surface thermometer at the job
site. - -False
-If solvent is trapped in a coating film it may - -cause problems with the curing of the
film.
-Electronic Surface Contact Thermometers - -do not require stabilization prior to use
-MOST coatings in the industrial and marine field are inorganic coatings? - -False
-The predominant pigment in sacrificial coating is - -zinc
-The vehicle of a coating consists of - -solvent, binder, and liquid additivess
-All of the following dissolve within the coating EXCEPT - -pigments
-Which coating type slows the penetration of oxygen, water, and soluble salts to form
electrolyte at the coating/metal surface? - -barrier coatings
-Mud cracking of an inorganic zinc-rich (IOZ) primer can be caused by - -applying the
coating too thick
-All of the following are commonly used as primers for steel structures EXCEPT - -vinyl
esters
-Convertible coatings cure by - -a variety of polymerization mechanisms
Questions with 100% Correct Answers |
Updated & Verified
All corrosion of iron at normal ambient conditions is - -an electrochemical process
-The cathode of a corrosion cell - -has an opposite electrical polarity to the anode
-Based on the galvanic series presented in the NACE CIP Level 1 Manual, which three
can be used effectively as galvanic anodes for carbon steel? - -Zinc, aluminum,
magnesium
-A corrosion inhibitor is a substance that, when added to an environment - -decreases
the rate of corrosion
-A decrease in temperature will generally cause the corrosion rate to - -decrease
-The electrolyte is the solution that carries (conducts) - -the anion, and the cations
-While oxidation occurs at the anode, reduction occurs at the cathode - -true
-The four elements of a corrosion cell are anode, the cathode, the electrode, and the
metallic pathway - -False
-The anode is the - -part of the metal that corrodes
-General corrosion is described as - -uniform loss of thickness over the exposed surface
-In order to reach consensus and to resolve conflict on the job, the NACE Inspector's
preferred course of action is to - -actively listen and endeavor to understand the
postions of others.
-A proper coating specification should contain information regarding - -surface
preparation standards, safety, locations to be coated
-According to the NACE attestation, it's OK to accept a gift from a contractor as long as
the gift is below the value identified in your company policy. - -false
-If an inspector finds discrepancies between the specification and the coating
manufacturers technical data sheet, the preferred coarse of action is to - -seek written
clarification from the specifier
-All of the following are generally included within inspection reports EXCEPT - -cost
information
, -Inspectors reports provide sufficient detail permitting the owner to evaluate - -
contractor's performance, inspector's performance, job progress, work interruptions
-When applying coatings, instruction regarding appropriate types of Personal
Protection Equipment (PPE) will always be found within the - -material safety data
sheet (MSDS) or safety data sheet (SDS)
-Material inventory report should contain all of the following EXCEPT - -overall cost of
materials
-Safety enforcement is one of the primary responsibilities of the coating inspector - -
false
-If the relative humidity is too high, solvent entrapment within the coating film may
occur. - -true
-The dew point is the - -temperature at which moisture condenses on a surface.
-Steel surface temperature reading should be taken - -at the actual work locations
-The coatings inspector must calibrate the magnetic surface thermometer at the job
site. - -False
-If solvent is trapped in a coating film it may - -cause problems with the curing of the
film.
-Electronic Surface Contact Thermometers - -do not require stabilization prior to use
-MOST coatings in the industrial and marine field are inorganic coatings? - -False
-The predominant pigment in sacrificial coating is - -zinc
-The vehicle of a coating consists of - -solvent, binder, and liquid additivess
-All of the following dissolve within the coating EXCEPT - -pigments
-Which coating type slows the penetration of oxygen, water, and soluble salts to form
electrolyte at the coating/metal surface? - -barrier coatings
-Mud cracking of an inorganic zinc-rich (IOZ) primer can be caused by - -applying the
coating too thick
-All of the following are commonly used as primers for steel structures EXCEPT - -vinyl
esters
-Convertible coatings cure by - -a variety of polymerization mechanisms