Pass
Temp range CUI on SS material
150-400
Fitness for service code
API 579
RBI code
API 580
API design for fabrication of exchangers
API 660
In service welding code
API 2201
Alternate evaluation for pits and LTAs
Section 8 div 2
Welder and weld procedure qualification
Section 9
NDE personnel qualification
ASNT SNT - TC - 1A
AIRR
Alteration, inspection, repair, rerate
JUIC
Jurisdiction, user, insurance company, contractor
AJOC
API 510 repair org - ASME stamp holder, authorized by jurisdiction, owner, contractor
How to determine corrosion rate for new or change in service
SPEC (same or similar service, published data, exam within 3-6 months, corrosion
specialist)
Primary responsibility of inspector
, TIRE (testing, inspection, repairs, examination)
Alteration
Physical change
Repair
Restore to suitable conditon
Two RBI primary factors
Probability and consequence
PRDs- requirements for relief device inspection
Qualified and experienced
PRDs - how relief devices intervals are determined
Performance
Maximum length of crack, IP or incomplete fusion allowed on a new weld
0"
Smoothness of RV seating surfaces
3 light bands
Maximum allowed mill tolerance for plate
Lesser of .01" or 6% of thickness
Maximum allowed size of open discontinuity in bend test
1/8"
Thickness for iridium 192
.25-3"
Distance beyond area of inspection for cleaning for MT/PT
1"
Minimum radius of insert patch
1"
Evaluate Lta. Distance from weld for E = 1.0
Greater of 1" or 2T
Thickness range of RT using cobalt 60
1.5-7
Wall thickness of a CS shell that requires PWHT
1.5"