A full lot of super pave asphalt is what size?
1,000 tons
1,000 to 2000 tons
2000 to 4000 tons
1 days production - ANS-2000 to 4000 tons
Which is not typically used as an asphalt binder in fdot mix designs?
PG 52-28
PG 58-22
PG 62-22
PG 76-22(PMA)
, PG 82-22 (PMA) - ANS-PG 62-22
Who cuts the density cores used for verification testing?
The verification technician
The contractor
The independent verification testing technician
None of the above - ANS-The contractor
A full lot is composed of 5 sublots and 4 cores per lot T/F - ANS-False
Given the target mix temperature of 290 degrees and the following truck temperatures 280, 285, 295,
300, 275....
No action is required, just document the results
Reject the load exceeding the master range temperature target
Check the next 5 loads to see if in tolerance and notify the plant - ANS-No action is required
What is the most important for consistent compaction of asphalt mix?
The mix is hotter in temperature
The mix is colder in temperature
The mix is uniform in temperature
Temperature of the mix does not affect compaction - ANS-The mix is uniform in temperature
Referring to general stationing guidelines, R1 would be ____ than R2
Closer to centerline
Closer to outside shoulder
Closure to the inside shoulder
Both A and C - ANS-Both A and C
While using the rolling straightedge, if the needle goes in the red zone indicating an unacceptable high
spot in the section, you then - ANS-Mark the pavement where the needle first goes into the red zone
and place another mark where the needle leaves the red zone and continue