100% Correct Answers | Updated & Verified
1. To measure the strength ofa welded joint what mechanical test would you
,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/
prescribe?
,/
a) A transverse weld tension test.
,/ ,/ ,/ ,/
b) A charpy test.
,/ ,/
c) A CTOD test.
,/ ,/
d) An all weld metal tension test.
,/ ,/ ,/ ,/ ,/
e) A side bend test.
,/ ,/ ,/
Ans:a) A transverse weld tension test.
,/ ,/ ,/ ,/ ,/ ,/
2. Select the cuttingprocess that would provide the narrowest heataffected
,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/
zone when cutting 12.5 mm (0.5 in) thick carbon steel.
,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/
a) Oxy-acetylene cutting. ,/
b) Air-carbon arc cutting. ,/ ,/
c) Oxy-propane cutting. ,/
,/ ,/
, d) Plasma arc cutting. ,/ ,/
e) Laser beam cutting ,/ ,/
Ans:e) Laser beam cutting
,/ ,/ ,/ ,/
3. Which of the following refers to a welder test where a pipe assembly is placed
,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/
vertically andthe joint welded inthe horizontalpositionwithout rotat- ing the
,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/
assembly?
,/
a) 1G
b) 2G
c) 3G
d) 5G
e) 6G
Ans:b) 2G
,/ ,/
4. Which of the following imperfections is normally considered as unaccept-
,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/
able regardless of size or location?
,/ ,/ ,/ ,/ ,/ ,/
a) Porosity.
b) Crack.
c) Inadequate penetration. ,/
d) Lamination.
e) Burn-through.
Ans:b) Crack.
,/ ,/
5. Select the correct penetrameter thickness for 2%sensitivity when radi-
,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/ ,/
ographing a weldment 1.25 inches in thickness.
,/ ,/ ,/ ,/ ,/ ,/ ,/
a) 0.012 in. ,/
b) 0.015 in. ,/
,/ ,/